Deep form mortars with lips are glazed on the outside (except for the bottom) and unglazed inside. Oversized pestles are glazed to grinding surface.
• Thermal Shock Resistance – average coefficient of expansion from 20 DEG C to 200 DEG C is 3.56 x 10-5, gradually increasing to 4.69 x 10-5 at 1050 DEG C. Every batch of porcelain is heat tested in our factory.
• Glaze – No softening occurs up to 1000 DEG C, and it is extremely white.
• Resistance to Chemical Action – Resistance to acids and alkalies is excellent, except for hydrofluoric acid.